POLYETHER POLYOL POUR MEUBLES SPONGE-POP
| Marque déposée | HPOP40 | POP36 / 28 | POP93 / 28 |
|
Indice d'hydroxyle
mgKOH / g |
20-23 | 25-29 | 23-27 |
|
Teneur en eau
% |
W 0.05 | W 0.05 | W 0.05 |
| pH | 6-9 | 6-9 | 5-8 |
|
Viscosité
mPa • s/25℃ |
W 6500 | W 3500 | W 3500 |
|
Du contenu solide
% |
39-41 | 23-25 | 26-28 |
|
La couleur
ICI |
|||
| Fonctionnalité | 3 | 3 | 3 |
| Masse moléculaire | 3000 | 5000 | 6000 |
| Application | High activity POP with solid content of 40 is used in preparation of high-load flexible polyurethane foam by mixing with high activity PPG. The hardening capability is higher than POP 36/28 and POP93/28. | High activity POP with solid content of 24 is used in preparation of high-load flexible polyurethane foam by mixing with high activity PPG. | High activity POP with solid content of 27 is used in preparation of high-load flexible polyurethane foam by mixing with high activity PPG. The hardening capability is higher than POP 36/28, but is less than HPOP 40. |
| Fonctionnalité | |||
| Note: please read the above information carefully and once you use the polyol in area that doesn’t involve in the mentioned scope,please consuit us first | |||